Applying Large Photo-etch Elements?

Got a question about techniques, materials or other aspects of physically building a model? This is the place to ask.

Moderators: DasPhule, Moderators

Post Reply
WarpeD
Posts: 8984
Joined: Mon Jul 15, 2002 9:00 pm
Location: Tucson, AZ

Applying Large Photo-etch Elements?

Post by WarpeD »

By the end of the month or early December, I'll have that 1/72nd Gato I've been looking forward to for rather a long time. I will also have all the Eduard photo-etch I need.

I just learned about annealing the stuff, and will certainly need to do that for this enormous boat.

But there are large swaths of brass intended to be laid in on the surface of the hull, and I don't want to fark this up.

What's the best, most forgiving, and most reliable means of applying large layer format photo-etch to a plastic surface of any kind?
User avatar
Kylwell
Moderator
Posts: 29643
Joined: Sun Nov 02, 2003 9:25 pm
Location: Lakewood, CO
Contact:

Post by Kylwell »

Rough & clean the glue surface and apply with a slower setting CA like Gorilla then clean up the over run with some debonder or acetone on a q-tip.

And clamps, LOTS of clamps. Quadruple check position.
Abolish Alliteration